After sericite was purified, the content of SiO2 decreased from 60.9wt% to 51.4wt%, and in the crystal phase the intensity of quartz decreased significantly. For the high grade purification of sericite, the removal of iron and separation of quartz for the raw ore (sericite), the hydrocyclone were used with the magnetic separator.